TECHNET Archives

April 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
quoted-printable
Sender:
Subject:
From:
Charles Caswell <[log in to unmask]>
Date:
Thu, 11 Apr 2002 14:54:21 -0500
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Charles Caswell <[log in to unmask]>
Parts/Attachments:
text/plain (46 lines)
I used to keep a bar of naptha soap in the restroom when I was working wave solder . Works for the rosin and the grease. Also good to take it out of clothes.
Charles Caswell
Process Lead, PCB
Frontier Electronic Systems 

-----Original Message-----
From: Jim Jenkins [mailto:[log in to unmask]]
Sent: Thursday, April 11, 2002 7:52 AM
To: [log in to unmask]
Subject: [TN] Hand cleaners


Hi everyone,

I know this may be a minor concern, but I get a lot of complaints from
operators that they have nothing that will get rosin flux residue off their
hands.  Some are very concerned about what the residue is doing to their
health.  Do any of you know of a good hand cleaner (especially one that
comes in an industrial size dispenser) that removes rosin flux?

Thanks and have fun,

Jim Jenkins

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2