TECHNET Archives

August 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 21 Aug 2003 10:31:47 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Yannick Brisson <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Yannick Brisson <[log in to unmask]>
Parts/Attachments:
text/plain (72 lines)
Hi, 

we'll use the cabinet for keep our QFP dry, we use to have a moisture
probleme right now, I don't know the level of humidity/dryness to be
maintained, cause it's maybe depending of the component, we don't what
something complex, jsut a standard cAbinet not to expensive...

Yannick


-----Message d'origine-----
De : Morse, Carrie [mailto:[log in to unmask]]
Envoyé : Thursday, August 21, 2003 10:26 AM
À : TechNet E-Mail Forum.; Yannick Brisson
Objet : RE: [TN] Dry Cabinet


Yannick,
What will you be using the dry cabinet for?
What level of humidity/dryness must be maintained?

Calibration, maintenance etc will depend on the unit you buy.

Let us know your application so we can give more info.

-Carrie

-----Original Message-----
From: Yannick Brisson [mailto:[log in to unmask]]
Sent: Wednesday, August 20, 2003 12:21 PM
To: [log in to unmask]
Subject: [TN] Dry Cabinet


Hi,

        Have someone ever work with dry cabinet?  We are thinking about
buying one and I don't know anything about it.  what should I look for? I
learn that the one for photography is cheaper than for electronic and do the
same job.  Do I need to plan some maintenace on it, calibration, is there a
used market for that what are the compagny who sold them.

  So many question...hehehe

Thanks You

Yannick

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2