Tom,
Well...all kinds of responses to this person's input come to mind,
and most of which might not be considered politically correct (a good
sized well-place ball pien hammer for instance,heh-heh). Anyway,
bottomside (glue) process has been around for MANY yeras, used by lots
of us folks, billions of boards. There are descent specs for It's use
in IPC-610B, etc. that may convince him. I am assuming a fair amount
of leaded joints is making the wave process very cost-effective. You
did not give a lot of specifics, but I would research the why's of the
one failure first, before throwing a process change in there...i.e., a
simple artwork change may solve the problem, without tooling costs &
process changes. If that is the only problem you had on such a small
first-time run, congratulations on a good first cut! Anyway, that's my
$0.02 worth.
Jeff Hempton
United Technology Electronic Controls
______________________________ Forward Header __________________________________
Subject: [TN] Wave solder VS Reflow on bottom side
Author: Thomas C Han <[log in to unmask]> at Internet
Date: 9/22/98 6:09 PM
Hi all
I have a mixed technology double sided board. It has about 900
components w/ 250 passive components on bottom. The total project is for
only 15 boards and 2 boards were manufactured for first article test.
Since the total account was for such small quantity I ran all 15 boards
thru SMT. The process was: top side reflow, bottom side epoxy, PTH
insertion, wave. Problem is that our customer found 1 solder short
across a cap on the bottom side, and so he is questioning my process of
epoxying the bottom side. Even though he is a manufacturing engineer, he
is not knowledgable in PCB assembly processes. How can I explane to him
that any failure in a component is wrong, but 1 out of 500 components( 2X
250 on bottom) is an acceptable figure that I do not see a need for
change. He insists that since his past CM used reflow and then a pallet
thru wave, that that is a superior process.
He also questioned the fact that solder short on that particular location
happened only to 1 board. And that if I took a systematic process, then
the solder short should exist on both boards.
Fellow Technetters, tell me how I can deal with such complaints.
Thanks for all your input.
Tom Han
Ardent Systems
_____________________________________________________________________
You don't need to buy Internet access to use free Internet e-mail.
Get completely free e-mail from Juno at http://www.juno.com
Or call Juno at (800) 654-JUNO [654-5866]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|