Hi Rudy,

Three points:

1. Electroless copper etches faster than base copper or electrolytic copper.

2. Watch for excessive overetching inner layers  (eg multiple passes etc)

3. Third formulation based on potassiumperoxomonosulphate also loved by
supply houses.

Best Regards,

Ken McGowan.
----- Original Message -----
From: "<Rudy Sedlak>" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, June 12, 2001 7:42 PM
Subject: Re: [TN] Sulfuric peroxide preplate microetch


> In a message dated 6/12/01 8:57:10 AM Pacific Daylight Time,
[log in to unmask]
> writes:
>
> Phil:  Happy to help, do be careful, you have made a coupla errors that
could
> have been dangerous if implimented....
>
> << What it the standard formulations for sodiium peroxide or ammoniun
peroxide
>  microetch
>
> You mean, Phil, Sodium or Ammonium PerSULFATE, (There exists Sodium
Peroxide,
> and you do not want to go near the stuff.....)
>
> Figure 8 oz/gal (60 grams/liter) Sodium Persulfate, which is preferred
over
> the Ammonium salt, because the Sodium Salt does not chelate, thus waste
> treats easily.  Add 1-2% Sulfuric Acid, you there.
>
>  and the sulfuric/hydrogen peroxide
>
> The big problem with sulfuric/peroxide is that the peroxide is inherently
> very unstable, and you gotta buy a proprietary additive to keep it stable,
> otherwise, things can get a little unstable as you introduce Copper into
the
> solution.
>
>   Also is the temperature elevated or at ambient temperture.
>
> Temp usually runs ambient to slightly elevated (under 100 F)  depending on
> spray or soak, immersion time, etc.
>   >>
> Rudy Sedlak
> RD Chemical Company
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2