TECHNET Archives

November 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Chuck Brummer <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 28 Nov 2012 10:54:23 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (245 lines)
Vic,

If I am oriented correctly as to what I am looking at I think you are 
looking at the end of a broken glass fiber that is protruding through the 
resin.

I forgot to mention earlier that a Tg and uTg spread should be only about 
3 to 4 degrees C to assure very good cure, 5 to 6 is okay.

Another thing to look at is peels before and after solder float.  If peels 
increase more than 10% after solder float cure is in question.

Chuck


Charles W. Brummer | 3M Manufacturing Engineer
3M Electronic Solutions Division
3M Canoga Park, 8357 Canoga Ave. | Canoga Park, CA 91304
Office: 818 734 4930
[log in to unmask] | www.3M.com


This message (including any attachments) may contain material, non-public 
information or proprietary information and is for the intended recipients 
only. If you are not the intended recipient, you should notify the sender 
and delete this message. Any disclosure, copying, or use of this 
information is strictly prohibited and may subject you to legal liability.



From:   <[log in to unmask]>
To:     <[log in to unmask]>
Cc:     <[log in to unmask]>
Date:   11/28/2012 10:18 AM
Subject:        RE: [TN] Delta Tg on a Pb-free board.



Chuck,

   Here is a photo of an laminate anomaly I want to understand.   The 
anomaly follows the glass rod arch.   I feel that the resin did not wet to 
the glass rod.   I am open to comments/suggestion/discussions.

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chuck Brummer
Sent: Wednesday, November 28, 2012 11:52 AM
To: [log in to unmask]
Subject: Re: [TN] Delta Tg on a Pb-free board.

Vic,

What makes you think the resin and glass stick to each other?  Having 
worked in a prepreg treater I can suggest that when they make this product 
a resin pump forces resin through the glass and coats both sides.  Once 
the resin is cured it sticks to itself surrounding the glass bundles and 
holding them in place.

I have my doubts that the resin to glass has much of a bond.

Chuck


Charles W. Brummer | 3M Manufacturing Engineer 3M Electronic Solutions 
Division 3M Canoga Park, 8357 Canoga Ave. | Canoga Park, CA 91304
Office: 818 734 4930
[log in to unmask] | www.3M.com


This message (including any attachments) may contain material, non-public 
information or proprietary information and is for the intended recipients 
only. If you are not the intended recipient, you should notify the sender 
and delete this message. Any disclosure, copying, or use of this 
information is strictly prohibited and may subject you to legal liability.



From:   Vladimir Igoshev <[log in to unmask]>
To:     <[log in to unmask]>
Date:   11/28/2012 09:08 AM
Subject:        Re: [TN] Delta Tg on a Pb-free board.
Sent by:        TechNet <[log in to unmask]>



One should keep in mind that the method doesn't specify a pass/fail 
number!?
Regards,

Vladimir

SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca

-----Original Message-----
From: Victor Hernandez <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date: Wed, 28 Nov 2012 10:55:11
To: <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>,
        <[log in to unmask]>
Subject: Re: [TN] Delta Tg on a Pb-free board.

Eric,

   Thanks for sharing.   This shared Test Method will test for laminate 
properly cures to specifications.   Now the question is. Is there a Test 
Method for evaluating  the woven fiber glass cloth adhesion property to 
the resin system,?

"X" 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Honsowetz, Eric
Sent: Wednesday, November 28, 2012 8:35 AM
To: [log in to unmask]
Subject: Re: [TN] Delta Tg on a Pb-free board.

IPC-TM-650 2.4.25

eric


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Wednesday, November 28, 2012 7:30 AM
To: [log in to unmask]
Subject: Re: [TN] Delta Tg on a Pb-free board.

Board guru,

   Is there a test method, IPC Standard, for testing how well a laminate 
has been cured, IS415.

"X"

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Zweig
Sent: Tuesday, November 27, 2012 4:11 PM
To: [log in to unmask]
Subject: Re: [TN] Delta Tg on a Pb-free board.

On Nov 27, 2012, at 4:46 PM, "Vladimir Igoshev. PhD" 
<[log in to unmask]> wrote:

> Hello board gurus,
> 
> We ran a DSC test on a Pb-free PWB and found that Tg1 was around 172C, 
> while the second heating produced Tg at about 185C. Below is a reply 
> from the board vendor, stating that there is no such a thing as 
> undercured laminate for that specific type of material.
> 
> I'd greatly appreciate any constructive comments.
> 
> "...That type of delta Tg would only apply to dicy materials when Tg1
and Tg2 are less than the advertised Tg of the material.
> EM-827 is a high Tg, filled phenolic and as such for these type
phenolics, there is no delta Tg that signifies undercure.
> With filled phenolics like this both the Tg1 and Tg2 would be under 
> the
advertised Tg to be undercure and this is not the case.
> As you cure more and more these type phenolics both Tg1 and Tg2 move 
> to higher and higher values and the delta Tg remains about the same".
> 
> 
> --
> Best regards,
> 
> Vladimir Igoshev. PhD 
mailto:[log in to unmask]
> 
> SENTEC Testing Laboratory Inc.
> 11 Canadian Road, Unit 7.
> Scarborough, ON M1R 5G1
> Tel: (416) 899-1882
> Fax: (905) 882-8812
> www.sentec.ca
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

**********************
** LEGAL DISCLAIMER **
**********************

This E-mail message and any attachments may contain legally privileged, 
confidential or proprietary information. If you are not the intended 
recipient(s), or the employee or agent responsible for delivery of this 
message to the intended recipient(s), you are hereby notified that any 
dissemination, distribution or copying of this E-mail message is strictly 
prohibited. If you have received this message in error, please immediately 
notify the sender and delete this E-mail message from your computer.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________
[attachment "Woven glass cloth glass ros anomaly-1.JPG" deleted by Charles 
W. Brummer/US-Corporate/3M/US] [attachment "Woven glass cloth glass ros 
anomaly-1a.JPG" deleted by Charles W. Brummer/US-Corporate/3M/US] 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2