Daniel,
Most flex cracks are hidden under the termination at the capacitor
termination/PWA interrface making it very difficult to detect using SLAM
or C-SAM. A quick way to uncover cracks is exposure to humidity & bias
accelerating failure. A few temp cycles ahead of humidity testing will
open the cracks a bit easing humidity entering the capacitor body
accelerating failure.
John Maxwell
>A good acoustic microscope should be able to find these cracks quickly and
>non-destructively. It is not a cheap tool, though, at $100k-$200k depending
>on the options.
>
>On Mon, 5 Jun 2006 10:11:04 -0400, Tempea, Ioan <[log in to unmask]> wrote:
>
>
>
>>Hi Technos,
>>
>>a never ending story, ceramic caps that crack, possibly due to
>>
>>
>depanelizing. The damage is not visible, unless the cap is cross sectioned.
>
>
>>Is there any testing, thermal cycling or something like that, that could
>>
>>
>show the damage real fast?
>
>
>>Thanks,
>>
>>Ioan
>>
>>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|