Graham,
There should be a note on the fabrication drawing that indicates that
all hole sizes are after plating unless otherwise specified. IPC-2221
provides guidance on how to select a hole size to meet a component lead
requirement which would be a finished hole size. The fabricator selects
a larger drill size to compensate for the amount of plating, or other
finish, in the hole.
Regards,
Gary
Graham Collins wrote:
> Hello TechNet
> A question about through-holes on a flex. We are having some debate about how to interpret a drawing.
>
> Specifically, if I have a drawing that says:
> 1) fabricate per IPC 6013 type 4
> 2) tin-lead plating shall be per IPC 2221, method optional
> 3) hole size is specified in the drill schedule as 0.028", plated, +- 0.003"
>
> Our debate is about the hole size after plating. Does the +- 0.003" apply to the solder coated hole, or is that a copper only size? Does IPC-2221 specify any maximum solder thickness?
>
> I'm an assembler, so unfortunately I don't have these two IPC specs at hand.
>
> regards,
>
> Graham Collins
> Halifax Production Engineering
> (902) 873-2000 ext. 6215
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|