TECHNET Archives

July 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
[log in to unmask], Leadfree Electronics Assembly Forum <[log in to unmask]>, TechNet <[log in to unmask]>
Date:
Tue, 24 Jul 2007 08:22:14 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Subject:
From:
John Burke <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<17FE4A8B0527604CA5E570ADBB03D408411064@exchgsrv>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (184 lines)
The link to the new exemption requests for round 7 of the new exemption
requests is here:

 

http://ec.europa.eu/environment/waste/rohs_7_consult.htm

 

It is also reached by clicking the 4th button from the home page of
http://www.rohsusa.com <http://www.rohsusa.com/> 

 

Kind regards,

 

John  Burke

 

 

 

John Burke

 

(408) 515 4992

  _____  

From: [log in to unmask]
[mailto:[log in to unmask]] On Behalf Of John Lau Hon-Shing
Sent: Monday, July 23, 2007 10:31 PM
To: [log in to unmask]; (Leadfree Electronics Assembly Forum);
TechNet
Subject: RE: [RoHSUSAPushback] Xbox 360 1 billion dollar reliability problem

 

Dear John:

 

Thank you very much for your speedy response. I agree with you that so far
no one got caught!

 

Now I have the other question which is about exemption. The 7th set of
exemptions is in the making (due August 10, 2007) and so far there are only
7 exemption proposals:

 

 
<http://circa.europa.eu/Public/irc/env/rohs_7/library?l=/induction-type_fluo
resce&vm=detailed&sb=Title> 1. Lead in silver rings on the exterior lamp
surface of induction-type fluorescent lamps.

 
<http://circa.europa.eu/Public/irc/env/rohs_7/library?l=/mercury_displays&vm
=detailed&sb=Title> 2. Mercury in plasma displays.

 
<http://circa.europa.eu/Public/irc/env/rohs_7/library?l=/photocells_equipmen
t&vm=detailed&sb=Title> 3. Cadmium in Photocells for accurate control of
lighting equipment.

 
<http://circa.europa.eu/Public/irc/env/rohs_7/library?l=/photo-resistors&vm=
detailed&sb=Title> 4. Cadmium-based photo-resistors used in professional
audio equipment.

 
<http://circa.europa.eu/Public/irc/env/rohs_7/library?l=/relock_fuse_x-09&vm
=detailed&sb=Title> 5. RELOCK FUSE, Model X-09.

 
<http://circa.europa.eu/Public/irc/env/rohs_7/library?l=/voltage_housings&vm
=detailed&sb=Title> 6. High voltage diodes in glass housings.

 
<http://circa.europa.eu/Public/irc/env/rohs_7/library?l=/beryllium_substrate
s&vm=detailed&sb=Title> 7. Cadmium and cadmium oxide in thick film pastes
used on beryllium oxide substrates.

 

Is this correct?

 

As always, thank you very much for your contributions and help!

 

John H. Lau

Microsystems, Modules & Components Laboratory

Institute of Microelectronics

11 Science Park Road

Singapore Science Park II

Singapore 117685

TEL:(65)6770-5424; [log in to unmask] <mailto:[log in to unmask]> star.edu.sg

 

 

  _____  

From: [log in to unmask]
[mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Tuesday, July 24, 2007 1:25 PM
To: [log in to unmask]; '(Leadfree Electronics Assembly
Forum)'; 'TechNet'
Subject: RE: [RoHSUSAPushback] Xbox 360 1 billion dollar reliability problem

Hi John,

I believe all "findings" are dealt with by warning the companies concerned
so that they "adjust" their product design.

I do not know of any general product that has been "caught" in the EU and
been made public as to the name of the company product type etc.

Kind regards,

John

John Burke

(408) 515 4992

  _____  

From: [log in to unmask]
[mailto:[log in to unmask]] On Behalf Of John Lau Hon-Shing
Sent: Monday, July 23, 2007 9:02 PM
To: [log in to unmask]; (Leadfree Electronics Assembly Forum);
TechNet
Subject: RE: [RoHSUSAPushback] Xbox 360 1 billion dollar reliability problem

Dear John:

Would you please tell me, as of today, is there any product get caught by
any of the EU countries?

Thanks & Best Wishes!

John H. Lau

Microsystems, Modules & Components Laboratory

Institute of Microelectronics

11 Science Park Road

Singapore Science Park II

Singapore 117685

TEL:(65)6770-5424; [log in to unmask] <mailto:[log in to unmask]> star.edu.sg


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2