Hi Rudy

We are using Cookson make No clean flux RF-800.Currently we are measuring
the specific gravity of the flux using Density meter.But I would like to
measure thru the titration method.Sujjest me the procedure for using the
titration method.

A.N.Prasad
Flextronics Technologies (I) Ltd.,
Bangalore, India
email:[log in to unmask]

* Flextronics Internal Use *


-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Monday, February 11, 2002 9:02 PM
To: [log in to unmask]
Subject: Re: [TN] Flux Testing using Titration


If you vendor will not give you a procedure..

Send me (off-line) your current procedure...

and I will work up a method, and send it to you.

Key issues needed to do this are:

Name of indicator...is flux water based, and do you add water during
testing?

Rudy Sedlak ([log in to unmask])

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2