It really "depends" and doesn't seem to have as much to do with
solderability as it does with the dreaded tin whiskers. We don't do
medical but we do some DOD and they are hell on tin whiskers and tin
finished component leads.
KennyB
-----Original Message-----
From: John Burke [mailto:[log in to unmask]]
Sent: Thursday, May 10, 2007 8:45 AM
To: [log in to unmask]
Subject: Re: [TN] PCB assembly for medical devices
WOW,
Before someone says "it depends" can I just point out that the medical
device manufacturer should be controlling the BOM and also should in
most
cases be requiring FDA tracking of the actual components used in the
assembly.
John
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of BADRI
Sent: Thursday, May 10, 2007 6:01 AM
To: [log in to unmask]
Subject: [TN] PCB assembly for medical devices
Dear All,
We have just started assembling some PCBA's to a medical device
manufacturer. They hate lead free. The question is as follows:
The components are leadfree and the paste used is leaded. Is it ok or do
I
have to pretin all the components with lead and then process.
We have processed couple of boards without pretinning and we have not
faced
any issue. Will the devise manufacturer accept it.
Please advise on the right process.
Advance thanx
Badri
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|