TECHNET Archives

July 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Date:
Mon, 2 Jul 2007 12:58:08 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Karen Ebner <[log in to unmask]>
Subject:
From:
Karen Ebner <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (139 lines)
Hi Dewey

This is great.  One question I have castellated parts.  How does this 
apply.  I need just a little help understanding this.

Any component which exceeds 7 grams in weight for every lead
of the device

Thanks.  Really appreciate your input!






"Whittaker, Dewey (EHCOE)" <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
07/02/2007 11:49 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] When to epoxy heavy components






Old Aerospace requirements are as follows:

*         Any component which exceeds 7 grams in weight for every lead
of the device

*         Any D case size components

*         Any odd geometry which could induce a high moment arm of
inertia

*         Any component which failed Qual( thermal cycling and
vibration) due to solder joint fracture or lead to body failure( broken
lead, package cracks, resistance increase)

There are other reasons to bond, but you requested heavy parts/ epoxy
bonding relationships.

Dewey

 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Karen Walters Ebner
Sent: Monday, July 02, 2007 8:13 AM
To: [log in to unmask]
Subject: [TN] When to epoxy heavy components

 

Sorry I am posting again but I was not subscribed.

 

I would greatly appreciate it if someone could help refresh my memory to


remind me of the golden rule on heavy components when to apply epoxy.
Phil 

Zarrow wrote an article on this some years back.

 

Greatly appreciate.

 

 

Karen Ebner

 

---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text
in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:
http://listserv.ipc.org/archives

Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815

-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2