Hopefully my lil nugget of info will help.....
FR-1-A low-grade version of FR-2.
FR-2-A NEMA grade of Flame-Retardant industrial laminate having a substrate
of paper and a resin binder of phenolic. It is suitable for printed circuit
board laminate and cheaper than the woven glass fabrics such as FR-4.
FR-4-A NEMA grade of Flame-Retardant industrial laminate having a substrate
of woven-glass fabric and resin binder of epoxy. FR-4is the most common
dielectric material used in the construction of PCBs.
FR-6- Fire-Retardant glass-and-polyester substrate material for electronic
circuits. Inexpensive; popular for automobile electronics.
Those wanting to be really "Geeked" up...Hopefully this will give a little
more insight: http://www.ilnorplex.com/quickref.htm
Regards,
Cal
Communications Test Design, Inc.
www.CTDI.com
-----Original Message-----
From: Jason W. Gregory [mailto:[log in to unmask]]
Sent: Wednesday, September 10, 2003 12:10 PM
To: [log in to unmask]
Subject: Re: [TN] FR-4
Jim
Right you are...."resistant". Maybe I'm retardant.
Jason Gregory
Jim Geer
<Jgeer@PRIME-MEASU To: [log in to unmask]
REMENT.COM> cc:
Sent by: TechNet Subject: Re: [TN] FR-4
<[log in to unmask]>
09/10/2003 11:08
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to Jim
Geer
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|