Dr. Doug Brooks published an article on this with the calculations called Fusing Current: When Traces Melt Without a Trace! You can get a copy of it at http://www.ultracad.com/article_outline.htm .
Jeffrey A McGlaughlin, CID
Engineering Designer
Battelle
505 King Ave
Columbus Ohio 43201-2693
Phone (614)424-7582
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of GRIVON Arnaud
Sent: Friday, September 05, 2008 5:44 AM
To: [log in to unmask]
Subject: [TN] PCB Trace Over-Current Withstanding Time
Hello all,
Is anyone able to answer the following query about PCB traces over-current
withstanding time : I am questioned about the existence of a plot giving the
with-standing time of PCB traces versus over-current.
Question is asked for 0.15mm up to 0.21mm line widths, 35µm/70µm thickness
and currents of 50A to 100A.
Any clue?
Best regards,
Arnaud Grivon
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|