Steve,
I suggest that you use oxygen plasma to decap plastic parts.  Works well.

Doug Pauls




                      Steve Gregory
                      <[log in to unmask]        To:       [log in to unmask]
                      m>                       cc:
                      Sent by: TechNet         Subject:  [TN] Plastic IC Decapsulation...
                      <TechNet@listserv
                      .ipc.org>


                      07/24/2003 08:56
                      AM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to
                      SteveZeva






Mornin' All!!

Been rather quiet on the list over the past week or so, hadn't it? Either
means everybody is on vacation, or everybody is so busy building stuff
without problems that they don't have any spare time...like to wish that
was the case.

Anyway, about Plastic IC Decapsulation, is that something I could do
myself? If so, what sort of chemicals would I use? Or is this something
better left to be done by the people who do that for a living, like failure
analysis labs?

Thanks!

-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2