TECHNET Archives

February 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vy3s6-0001ceC; Fri, 21 Feb 97 16:55 CST
Old-Return-Path:
Date:
Fri, 21 Feb 1997 16:23:58 -0500 (EST)
Precedence:
list
Resent-From:
From [log in to unmask] Fri Feb 21 17:
07:43 1997
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/10451
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"XNGqK2.0.A4A.BVY3p"@ipc>
Subject:
From:
X-Loop:
Message-ID:
Parts/Attachments:
text/plain (28 lines)
Attn CBH,

     One thing you didnt specify was the diameter of these rings. We have
also made this
'defect' while vacuum laminating Vacrel.  We have narrowed it down to pin
holes in the
mask itself, possibly from the manufacturer but most likely they were caused
by your
handling process. If while handling you so much as "crinkle" or 'pinch" the
material you
are likely to cause damage to the emulsion in that area and this ' fisheye'
will occur.


Brett 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2