TECHNET Archives

July 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Lee parker <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Lee parker <[log in to unmask]>
Date:
Fri, 20 Jul 2007 16:41:40 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (90 lines)
David

I always advise one mil or more in the PTH. Given the non-uniformity often 
seen in the PTH I would also spec the drill quality and the ratio of the 
copper at the top of the hole and in the center.

Best regards

Lee

J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389


----- Original Message ----- 
From: "David Harman" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, July 20, 2007 4:23 PM
Subject: [TN] Question on plated through holes general


I have a quick question and our standard that we have maybe an older
one. We currently use the ANSI/IPC-A-600 Rev E





Page 70   Micro section:



There is a table describing copper plating thickness min, requirements





                                                Class 1
Class 2                         Class 3

Average Min Thickness              .020mm (0.0008in)        0.025mm
(0.001 in)       0.025 mm (0.001 in)



Minimum this area                     .0015 mm( .0006 in)       0.020 mm
(.0008 in)     0.020mm  (.0008 in)







Can anyone tell me if this still is a current standards for  copper
plating thickness measurements.



David Harman




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
----------------------------------------------------- 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2