TECHNET Archives

June 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Igoshev, Vladimir" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Igoshev, Vladimir
Date:
Wed, 18 Jun 2008 17:00:29 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (58 lines)
Hi Werner,

 

I agree, strictly speaking that is how it should have sound.

 

I put it the way I did because I'd have hard time imagining how badly
the laminate material had to be "screwed" to have the UTS value close to
almost 0, as that would be the case for a BP affected joint. :-)

 

Regards,

 

Vladimir 

 

________________________________

From: [log in to unmask] [mailto:[log in to unmask]] 
Sent: Wednesday, June 18, 2008 4:55 PM
To: Igoshev, Vladimir; [log in to unmask]
Subject: Re: [TN] [LF] [TN] SN100 for Reflow Application

 

Hi Vladimir,
You say: "The fact that you also got cracks in laminate rules out
BP"-not so. It just means that the resin cohesion and the interfacial
adhesion are about equally weak.



Werner



**************
Gas prices getting you down? Search AOL Autos for fuel-efficient used
cars.
(http://autos.aol.com/used?ncid=aolaut00050000000007)


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2