Pete,
Before you try the Dow "OS-2", let me tell a little story. This material works by causing the
silicone to expand, to the point where is looses its grip.
I had an engineering prototype of a small sensor assembly that the design guys wanted stripped
of coating for some reason or another. So, I let the assembly sit submerged in some OS-2 for
5-10 minutes. I then removed the assembly and brushed off the loose coating. After repeated
the process a couple of times I had removed the vast majority of the visible coating, but
there was still some coating under the components. I figured I would just let the assembly
sit in the OS-2 overnight. When I pulled the assembly out the following morning, the silicone
had expanded enough that it popped every SO-8 and SO-14 right off the board. The silicone had
developed enough force under the parts to pull the legs right out of the solder fillet.
Gary Camac
"" wrote:
> Hi, TechNetters,
>
> I am trying to find a solvent for removing 3M's RTV 738 that has been used
> for bonding components to a number of boards, or to each other. Any
> suggestions?
>
> I have tried 3M themselves and they have no solvent of their own apart from
> "Citrus Base Adhesive Remover" that 'may soften' it enough to peel it off,
> but this seems pretty indefinite.
>
> Thanks in hope
>
> Pete Duncan
> Asst Principal Engineer
> Singapore Technologies Aerospace
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|