Further FYI:
John Burke reported that the Sodium or Potassium converts to the Hydroxide salt when contacted by water. However, they are not commonly found in saponifiers, BECAUSE these salts are known to attack Tin. Common reaction is this
KOH(Potassium Hydroxide) + Sn(Tin) + Water -> KSnO3 (Potassium Stannate, very water soluble)
This opens the possibility of cleaning solutions attacking the remaining Tin, and leaving it looking leached, or at least not shiney. Won't this cause some heated customer/vendor exchanges?
Rudy Sedlak
RD Chemical Company
John Burke <[log in to unmask]> wrote:
Just an FYI,
My regular Circuits Assembly column on lead free is at this link:
http://circuitsassembly.com/cms/content/view/4665/95/
There are some interesting developments in lead free soldering covered.
Kind regards,
John Burke
John Burke
(408) 515 4992
---------------------------------
Get your own web address.
Have a HUGE year through Yahoo! Small Business.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|