TECHNET Archives

November 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Rod Semen <[log in to unmask]>
Date:
Tue, 23 Nov 1999 08:39:33 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Chuck Brummer <[log in to unmask]>
Subject:
From:
Chuck Brummer <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
Organization:
acuson
MIME-Version:
1.0
Parts/Attachments:
text/plain (103 lines)
Hey, take it easy.  Rudy is a rep, but he gives lots of GOOD, FREE advice. There is no
valid reason to be rude, we all know he sells for a living.  Take the chip off your
shoulder and limit yourself to helpful advice.

Chuck Brummer
I don't sell anything!

Rod Semen wrote:

> Hey Rudy,
>
> Next time buy an ad! If this is not thoses blatant advertising post, then I
> do not know what is. And by the way I have used your resist stripper.
> It sucked.....
>
> >From: Rudy Sedlak <[log in to unmask]>
> >Reply-To: "TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
> >To: [log in to unmask]
> >Subject: [TN] Tarnish after resist stripping
> >Date: Tue, 23 Nov 1999 09:37:28 EST
> >
> >I do love it when someone asks a question that we are real knowledgeable
> >on.
> >Thank you.
> >
> >Tarnish on Copper after stripping is endemic to resist stripping.  It is
> >made
> >much worse by buildup of Copper in the stripping chemistry.  In other
> >words,
> >most strippers will not tarnish when new, but begin to tarnish as they are
> >used, and Copper builds in the sump.
> >
> >The problem is cureable by using a  resist stripping chemistry with the
> >proper anti-tarnish in it.  Most resist stripping chemistry has 250 ppm of
> >Copper when the stripper is dumped.  It is possible to get resist strippers
> >that will not build up more than 30 ppm of Copper for the same number of
> >panels stripped, and average less than 2 false defects per 18" X 24" panel.
> >This has a nice added benefit of keeping the Copper in the rinse waters so
> >low that they usually do not have to be treated, and can legally be put
> >right
> >down the drain.
> >
> >Many stripper chemistry vendors have resolved this issue by simply going to
> >high volume feed and bleed, thus turning the sump over often, and keeping
> >the
> >dissolved Copper levels low.  This is great for the chemistry vendor, but
> >expensive for the PCB fabricator, and not required with the proper
> >anti-tarnish chemistry.
> >
> >As you probably have surmised, we are one of the vendors who can supply
> >resist strippers with the proper anti-tarnish properties.
> >
> >Rudy Sedlak
> >RD Chemical Company
> >[log in to unmask]
> >
> >##############################################################
> >TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> >##############################################################
> >To subscribe/unsubscribe, send a message to [log in to unmask] with following
> >text in
> >the body:
> >To subscribe:   SUBSCRIBE TECHNET <your full name>
> >To unsubscribe:   SIGNOFF TECHNET
> >##############################################################
> >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> >additional
> >information.
> >If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> >847-509-9700 ext.5365
> >##############################################################
>
> ______________________________________________________
> Get Your Private, Free Email at http://www.hotmail.com
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2