TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 3 May 2006 07:12:44 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Barry Gallegos <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Barry Gallegos <[log in to unmask]>
Parts/Attachments:
text/plain (54 lines)
I would like to thank all for their input on this.
That is exactly what I was looking for.
Once again this forum is outstanding.

Barry

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Joe Fjelstad
Sent: Tuesday, May 02, 2006 4:57 PM
To: [log in to unmask]
Subject: Re: [TN] Thieving


In a message dated 5/2/2006 2:23:34 PM Pacific Daylight Time,
[log in to unmask] writes:

Am  looking for a definition of Thieving when applied to PCB  fabs.




Hi Berry,

In some cases it refers to the practice of nasty curs who make  off with gold
scrap and other valuables late at night... ;-)

But I believe that you are asking about non functional areas of the circuit
that are patterned to even out current distribution so that plating is more
uniform, a fairly common practice.

Kind regards,
Joe


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2