TECHNET Archives

April 2015

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 24 Apr 2015 13:04:27 -0400
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="UTF-8"; format=flowed; delsp=no
From:
Patrick Goodyear <[log in to unmask]>
Parts/Attachments:
text/plain (88 lines)
Phil,

I forgot to add when we do spot de fluxing we use a bundle of Q-tips or 
similar to absorb the washout in specific areas, so as not to spread it. 
Pace actually makes a tool, looks like a chalk holder that holds a 
sponge for dabbing up the residue after spot de-fluxing.

pat


On Fri, Apr 24, 2015 at 9:31 AM, Nutting, Phil wrote:

> Ok, so if I am spot washing flux off a circuit board or cleaning the 
> face of an epoxy insulator to remove silicone dielectric grease what 
> am I supposed to use?
>
> Brian,  I know you are very environmentally concerned.  IPA and the 
> like have been used for years by our industry and it is usually the 
> default cleaner for everything.  And yes I know alcohols do a better 
> job of spreading contaminates than removing them.  What then, if spot 
> cleaning, should be used?  (I know, "it depends".)  Manufacturing is 
> always complaining that Engineering creates designs and processes that 
> take too much time, but they work if done as designed.  Finding a 
> practical solution and changing the mindset is no small task.
>
> I look forward to your sage wisdom.
>
> Phil
>
> -----Original Message-----
> From: Brian Ellis [mailto:[log in to unmask]] Sent: Friday, April 24, 2015 
> 12:18 PM
> To: TechNet E-Mail Forum; Nutting, Phil
> Subject: Re: [TN] methanol for cleaning
>
> Yes! absolutely! And it is highly toxic, to boot, with ingress to the 
> body by all means, including cutaneous. IMHO, avoid it!
>
> Brian
>
> On 24/04/2015 18:12, Nutting, Phil wrote:
>> We have had many posts regarding the ability of alcohol to evenly 
>> distribute flux and other contaminates over the surface of the board 
>> or part.  Does methanol do that same thing?
>>
>> Phil Nutting  |  HVP Development Engineer   |  Excelitas Technologies 
>> Corp
>>
>> Lab: +1 978.224.4332   |  Office: +1 978.224.4152
>> 35 Congress St, Salem, MA  01970 USA
>> [log in to unmask]<mailto:[log in to unmask]>
>> www.excelitas.com<http://www.excelitas.com/>
>>
>>
>> [Excelitas R_emailsig]
>>
>>
>> Please consider the environment before printing this e-mail.
>> ________________________________
>> This email message and any attachments are confidential and 
>> proprietary to Excelitas Technologies Corp. If you are not the 
>> intended recipient of this message, please inform the sender by 
>> replying to this email or sending a message to the sender and destroy 
>> the message and any attachments. Thank you.
>>
>>
>> 
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud 
>> service.
>> For more information please contact helpdesk at x2960 or 
>> [log in to unmask]
>> 
>> ______________________________________________________________________
>>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud 
> service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2