Joe Fjelstad <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 17 Feb 2009 12:25:09 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (149 lines)
Hi Denny
 
We need Cr3 in our diets as an aid in glucose metabolism,  the same  case, 
cannot be made for lead. As for the lead industry lack or response, with  lead 
in solder representing less than 0.5% of all lead used annually, there was  not 
enough there to for them to worry about, on the other hand the increased use  
of tin was very beneficial to that industry and would provide ample incentive 
to  have lead in solder blackballed, whether or not they actually ever did  
so is known only for certain by the leaders of tin industry.  ( with  the word 
leaders obviously pronounced "leeders" not "leders"...  ;-)  

Cheers, 
Joe
 
 
In a message dated 2/17/2009 8:30:57 A.M. Pacific Standard Time, DDFRITZ  
writes:

My  ancient chemical engineering degree stirs me to comment on this thread 
(always  dangerous)

The main culprit in lead uptake by all animals is the  chemistry of the lead. 
 Oxidized state lead - lead oxide left from  burning leaded gasoline, or lead 
chromate from the various yellow, orange and  red lead pigments in paints is 
very easy for the blood to pick up.   Tetraethyl lead for leaded gas is 
horribly toxic to all animals because it is  so very easy to absorb (remember 
washing grease off your hands with gasoline  before about 1970?).  That ionized lead 
is still out there in the paint  chips or soil surface layer, as Joe points 
out.  

Elemental lead  is pretty innocuous to animals (carrying a bullet from the 
war, etc.) except  for one nice way to create ionic lead in the body - the 
stomach acid that  works on elemental lead when eaten.  That is not very fast, but 
it is  steady  - in the case where the lead remains in the stomach - ducks 
whose  gizzards grind shot or sinkers against sand and gravel in digestion, 
someone's  cow where the weight stayed at the bottom of one of the four stomachs, 
or  sadly, some super cheap lead trinkets that lodged in small child stomachs 
or  intestines.  Don't forget the cheap yellow and orange paint on toys  - we 
covered that before.   

I think years ago on TechNet, we  discussed how much lead is absorbed from 
lead solder assembly - I can't  remember a single case of significant lead fumes 
- am I wrong?  Sanity  says to ventilate - the flux smell can get to you.  I 
hear about lead  exposure from "roasting circuit boards on an open fire" in 
third world  countries.  How much of that is no hand washing instead of  
breathing?  How much from using the same pot for stir fry as for roasting  boards?

How did we get the environmentalists to limit chrome  controls to Chrome +6?  
A better marketing job by the "Chrome Industry  Council"?.  Lawmakers still 
wanted their shiny cars and plumbing  fixtures?  The stainless steel folks 
drove some sanity?  Guess there  is no "Lead Industry Council" to stand up for 
their product.  

My  simple answer would be to restrict lead where it is ionic (done now 
through  these bans), AND elemental lead where it can easily be ingested - shotgun  
shot, sadly for me fishing sinkers, and anything say smaller than 2  ounces.  
And, in my opinion, lead in solder for circuit boards is safe -  who eats 
them?  I think IPC helped get circuit boards in toys exempted  from this 
legislation, right?

What da ya think?
Denny  Fritz


-----Original Message-----
From: Joe Fjelstad  <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, 17 Feb 2009  10:49 am
Subject: Re: [TN] Leadfree has gone too far.


Unfortunately, the road to perdition is paved with good intentions  and it's  
sad to say, but common sense is not so common anymore. I am  confident that 
 there are many folks out there paving the road who are applauding  this 
news.  
 So it goes...
  
 Joe
  
 PS Steve's observations are on target. The lead acetate (aka lead  sugar) in 
 paint is what make eating paint chips attractive to children. The  
elimination 
 of lead from gasoline and paint were two of the best solutions  to reducing 
 lead in the environment. Others have  followed wanting to build on that 
legacy 
 using assertion without proof and  conjecture rather that science or data. 
For 
 the record, the  discovery of the fall out from lead in gasoline came when 
 there was a study  done to see if there was risk from using tin-lead solder 
for 
 canned food  lids which was shown to account for a smaller percentage than 
 expected. The "no  effect" limit for lead consumption is 3 mg per person per 
 
 week  according to "Encyclopaedia of Environmental  Agricultural Pollution 
and 
 Its Control" By G.R. Chhatwal.  in Chapter 21 "The Impact of Inorganic Spoil 
 Pollutants on Consumers" (but it  was not recommended ;-) 
  
 He also pointed out lead paint  licking by animals as one of the prime 
 sources and reported in the  book that higher calcium intake significantly 
 reduced 
 lead  uptake/absorption. Interestingly, most of the lead comes from the  
soil 
 attached to the roots eaten by grazing animals. Given the fact  that a micro 
 thin layer of lead has been deposited all over the land  over for the half 
 century that leaded gasoline was most common,  it reinforces the validity of 
the 
 
 ban (though it is  still in use for some aviation fuel and in some less 
 developed countries I  believe)
  
  
  
  
 In a message dated 2/17/2009 6:12:25 A.M. Pacific Standard Time,  
 [log in to unmask] (mailto:[log in to unmask])  writes:
 
 The kid in the  picture might accidentally eat the battery terminals. I
 just had to  laugh.
 
 _http://www.startribune.com/local/39693797.html?elr=KArksLckD8EQDUoaEyqyP_ 
(http://www.startribune.com/local/39693797.html?elr=KArksLckD8EQDUoaEyqyP) 
 4O:DW3ckUiD3aPc:_Yyc:aULPQL7PQLanchO7DiUss
 



 
____________________________________
A Good Credit Score is 700 or Above. _See  yours in just 2 easy steps!_ 
(http://pr.atwola.com/promoclk/100126575x1218822736x1201267884/aol?redir=http://www.
freecreditreport.com/pm/default.aspx?sc=668072&hmpgID=62&bcd=febemailfooterNO6
2)  


**************You can't always choose whom you love, but you can choose how 
to find them. Start with AOL Personals. 
(http://personals.aol.com/?ncid=emlcntuslove00000002)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2