Gregg,
what's the issue(s). We have been using QFNs for a long time and without
significant problems. However, as a microwave application guy (sometimes)
I'll give you two winks:
1. Have a hard look at your supplier's QFN center pad finish!
2. Correct solder paste volume for the center pad!
Here is a good microwave page, if you don' t already have it.
http://www.mwee.com/202803709
By the way, it's remarkable with the engineering life. Bumble-bees can' t
fly according to technical calculations. But she doesn' know that and is
flying since millions of years without any improvements. QFNs may be the
same ?
Inge
>
>
> To
> [log in to unmask]
> cc
>
> Subject
> [TN] Use of QFN devices in high reliability applications
>
>
>
>
>
>
> Our team is working on several new electronic devices whose application is
> primary, flight critical hardware for commercial aircraft.
>
> Our initial component selection includes many QFN packaged devices
> (leadless, bottom side termination only) which will be mounted on .063"
> FR4 boards using SN63. The devices range from 20 to 44 terminations.
>
>>From studies that are available on the web, a picture has emerged that QFN
> packages have reduced long term solder joint reliability when compared
> with leaded or some of ball grid array devices. Board thickness, flexing
> and whether the device has a central solderable heat sink seem to have a
> significant affect on reliability. Problem is there are no absolute
> numbers, so for critical applications it seems that thorough testing is
> required. We'd rather not wait until the end of a lengthy test regimen to
> find we've gone down the wrong path. Is there newer information
> abbailable? Two of the studies stated that further testing was being
> performed to support the reliability requirements for aerospace and other
> high-rel applications however I cannot find any updated information on the
> web.
>
> We have decided to replace several of the QFN's with leaded devices,
> however there are no direct crosses for 3 of the devices. One of them will
> require a number of components to create the same function; possibly an
> additional circuit card.
>
> Is anyone aware of information or recommendations that would be useful for
> our assessment? Is there any specific information that would drive us to
> use or not use them?
>
> Thanks for your help
>
> Gregg
>
>
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|