TECHNET Archives

June 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Phillips, Peter (NM05)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 15 Jun 2000 11:17:33 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (73 lines)
For what it's worth, here is an example of how one of our company's
divisions specifies laundering guidelines for ESD Smocks, Jackets, etc.:
Cleaning Instructions
Soiled Smocks and Conductive Drop Cloths may be laundered as follows:
Wash separately in machine set on gentle cycle using liquid TideŽ.
Hang and allow to air dry.  Do not use clothes dryer to dry.  Do not twist
or wring to remove excess water.

                          Honeywell
Peter A. Phillips, Sustaining Engineer
Manufacturing Engineering
Home and Building Controls
8500 Bluewater Road N.W.
Albuquerque, NM 87121-1958
Pho     505-831-7509
Fax     505-836-4834
[log in to unmask]

> The information in this electronic mail message is confidential and is
> intended only for the addressee(s) listed above.  It may also contain
> privileged information.  If you are not the intended recipient, do not
> read, copy, use or disclose this communication to others.  It is
> requested that you notify the sender of any mis-delivery by replying
> to this message, then delete it from your system.
> Thank you.


-----Original Message-----
From: Bob Perkins [mailto:[log in to unmask]]
Sent: Wednesday, June 14, 2000 12:04 PM
To: [log in to unmask]
Subject: [TN] ESD Coats


On the subject of ESD coats, I have heard that depending on the way you wash
and dry them you can take ESD safety right out of them.  Does anyone have a
proven procedure on the safest way to go about this.  i.e.. I heard dry
cleaning is a definite no-no.

Bob Perkins
Aimtronics-Delta
Automation Technician /
SMT Manufacturing Engineer

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2