TECHNET Archives

June 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wdEmY-000BjMC; Sun, 15 Jun 97 07:51 CDT
Old-Return-Path:
Date:
Sun, 15 Jun 1997 09:02:01 -0400 (EDT)
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
From [log in to unmask] Tue Jun 17 11:
18:10 1997
X-Mailing-List:
<[log in to unmask]> archive/latest/13421
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"ifuz41.0.N77.XL-ep"@ipc>
Subject:
From:
Status:
O
Message-ID:
X-Loop:
>From willli Sun Jun 15 07:
52:07 1997
Parts/Attachments:
text/plain (27 lines)
topic of Pd seems to be very interesting these days - everyone is looking at
it - at a glance. Please take note that there is a difference in a plated Pd
deposit - and an electroless Pd deposit. Electroplated Pd - has the inclusion
of organic additives that plate with the deposit, electroless Pd doesn't.
There is a paper written by IBM in the 97 IPC Expo proceedings that i think
could answer a lot of questions - but i know that in speaking with the
circuit manufacturers - they are not making a distinction between the two
type of deposits - while the board designers - or OEM's as they are called -
are. Majority of OEM's have done a lot of in-house studies - the fabricators
have not.

Regards

Richard Fudalewski
Atotech Canada Ltd

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2