Sender: |
|
X-To: |
|
Date: |
Mon, 12 Jun 2006 16:23:02 -0700 |
Reply-To: |
|
Subject: |
|
From: |
|
Content-Transfer-Encoding: |
quoted-printable |
In-Reply-To: |
|
Content-Type: |
text/plain; charset="iso-8859-1" |
MIME-Version: |
1.0 |
Parts/Attachments: |
|
|
That’s funny, most people were wondering why Monday afternoon was so far
from Friday looking forwards and such a short time ago looking
back........and the balance of the group was wondering whether they could
get away from their desks to catch the end of happy hour................8-)
I am sure the group will give you a serious answer, I am just working up for
Friday...........8- )
John
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Adam Seychell
Sent: Monday, June 12, 2006 4:03 PM
To: [log in to unmask]
Subject: [TN] cuprous ions in ammoniacal chloride etching
I am wondering if there is a simple test for cuprous ions in ammoniacal
chloride alkaline etching, and thus determine when to increases or
decrease the air ventilation intake of the etching machine. I am brewing
my own chemistry based on typical operating parameters of ammoniacal
chloride etchants.
Copper 2 ~ 2.5 Molar
Chloride 4.5 ~ 5 Molar
pH 8.0 ~ 8.6
Temp. 40 ~ 45 °C
I discovered just like with acid cupric chloride etching, that when the
cuprous content reaches to even small concentrations then the etch rate
is severely affected. In the lab, I tested as little as 5g/L of
dissolved copper in the cuprous state will slow etch rate, and at 10 g/L
it becomes virtually a stand still. For acid copper chloride etchants,
the loss of its bright green color is a quick indicator of cuprous ions
being present, and even 0.5 g/L will show beginnings of color change.
However in alkaline etching the cuprous ions do not appear visible or
change the solution color. I have heard about ORP (oxidation-reduction
potential) probes used in acid cupric chloride machines. Can these same
probes be used in ammoniacal chloride etchants ?
My chemistry is a bit poor, although I'm wondering if is possible to
make such a probe, using a standard reference electrode (e.g Ag/AgCl )
and a piece of copper wire as the indicator electrode.
Adam Seychell
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|