TECHNET Archives

April 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Mark Hargreaves <[log in to unmask]>
Date:
Fri, 9 Apr 2004 07:38:23 -0400
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Mark Hargreaves <[log in to unmask]>
Parts/Attachments:
text/plain (80 lines)
Morning Steve,
You could try throwing the book at them.

IPC-D-275,
Par 5.5 Coatings and Markings
"Coatings & markings shall be compatible with each other".
Par 5.5.1 Solder Resist Coatings
"Solder resist adhesion to melting metal surfaces (solder coating, tin/lead
plating, etc.) cannot be assured as boards are subjected to temperatures
that cause redistribution of the melting metals. ..............When solder
resist is required over melting metals, the maximum recommended conductor
width shall be 0.050".

Regards,
Mark
PS..Par 5.5.1 contains additional info.

        -----Original Message-----
        From:   Steve Gregory [SMTP:[log in to unmask]]
        Sent:   Thursday, April 08, 2004 9:52 PM
        To:     [log in to unmask]
        Subject:        [TN] Solder Mask over Tin/Lead...

        Had a really frustrating conference call today. Our customer is
standing firm
        that they will not change their drawings on their fabs that specify
that
        everything needs to be coated with tin/lead before solder mask.

        Their arguement is that they've never had any problems before, so
why should
        they change anything...and I percieved that they blamed our assembly
processes
        for the mask adhesion issues that we were seeing.

        What do you do in a situation like this? I'm trying to gather as
much
        information as I can that shows that anything other than SMOBC is
risky, but during
        the conference call, anything that I tried to say was
dismissed...because they
        say that they've been doing this for years, and this is the first
time that
        they have heard from any of their subcontractors that there is a
problem.

        I suppose that there won't be any good answers for this, we'll have
to deal
        with this the best that we can. Sure makes life interesting...the
customer is
        always right, and we're all about customer satisfaction.

        -Steve Gregory-

        ---------------------------------------------------
        Technet Mail List provided as a service by IPC using LISTSERV 1.8e
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
        To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
        Search the archives of previous posts at:
http://listserv.ipc.org/archives
        Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
        -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2