TECHNET Archives

June 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 30 Jun 2004 13:11:29 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="US-ASCII"
From:
"Victor G. Hernandez" <[log in to unmask]>
Parts/Attachments:
text/plain (24 lines)
Fellow TechNetters:

    What is a rule of thumb for Thermal Heat Sink Spreader solder fillet
coverage.   During x-ray imaging I have observed varying coverage with
respect to the PCB copper
pad foot print and the heat sink.   This ranges from 30 to 90% coverage.
I am unable to state the associated thickness of this coverage except
for gray scale keeping all setting alike.   IPC does have a guideline
for PTH Vertical fill of 50% for Powers and 75% for signals.

   Can anyone share their experience with me.

Victor,

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2