TECHNET Archives

November 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Victor Hernandez <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 16 Nov 2012 10:06:44 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (23 lines)
Fellow TechNetters:

   Are the above artifact cause by the wettability of the resin to yarn, woven glass cloth rods, interface?   Then this artifact is enhance by mechanical stress.   I am trying to understand the terminology so that it is not misused.

"X"

From: Hernandez, Victor G
Sent: Friday, November 16, 2012 7:14 AM
To: TechNet E-Mail Forum ([log in to unmask])
Cc: Hernandez, Victor G
Subject: Laminate, Resin recession-dry glass bundle

Fellow TechNetters:

   Can any of the gurus out there comment on the above terminology and perhaps share a photo.   What is the worse than can occur within the laminate with such artifacts.

"X"

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2