TECHNET Archives

October 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Goodyear, Patrick" <[log in to unmask]>
Date:
Mon, 17 Oct 2011 12:40:11 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Garcia, Rigo (GSFC-300.0)[MANTECH SRS TECHNOLOGIES]" <[log in to unmask]>
Message-ID:
Subject:
From:
"Garcia, Rigo (GSFC-300.0)[MANTECH SRS TECHNOLOGIES]" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (55 lines)
Hi Pat,

You never hand solder a BGA. There are so many issues related to it that you will likely run into reliability problems (e.g. infant mortality). We use something similar called CCGAs (solder columns instead of solder balls) which provide a better level of long-term reliability than BGAs.

Check this document if you want to learn about the thermal and process issues of soldering these components (BGAs have very similar issues): https://www-01.ibm.com/chips/techlib/techlib.nsf/techdocs/630AFA7BD7DE3FED87256C0100558D50/$file/ccga.pdf

I hope this helps.

Rigo

Sr. Quality Assurance Engineer
Workmanship Standards, Code 300 
NASA, Goddard Space Flight Center
Greenbelt, MD  20771
Phone. (301) 286-6129
Fax.       (301) 286-6576


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Goodyear, Patrick
Sent: Monday, October 17, 2011 1:10 PM
To: [log in to unmask]
Subject: [TN] Reflow of BGA

Ok gang, I'm stretching my limits here.

Does anyone have experience with hand reflow of BGA?    I have never tried it.    Does one use a hot jet or can it be done with the iron to the component.
Most notably on a SODIMM, one of the memory chips has a bad connection, looks like 3 rows per side of 8 per row.

Pat


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2