TECHNET Archives

March 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 25 Mar 2016 08:49:09 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Wettermann <[log in to unmask]>
Subject:
From:
Bob Wettermann <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (61 lines)
The parts are roughly 9mm x 3mm x 1.5mm.

Do not know the end game (yet)

Bob
---------- Forwarded message ----------
From: Dennis Fritz <[log in to unmask]>
Date: Fri, Mar 25, 2016 at 8:45 AM
Subject: Re: [TN] Calling All Metallurgists
To: [log in to unmask]


Better give TechNet the underlying metal.  Chemicals that strip gold (and
other elements) frequently attack the underlying metal even faster than
they remove the gold.  Also, many of the chemical strippers contain cyanide
and are pretty dangerous.  Finally - what is size of part - dip in a beaker
or need a 55 gallon drum?


-----Original Message-----
From: Bob Wettermann <[log in to unmask]>
To: TechNet <[log in to unmask]>
Sent: Fri, Mar 25, 2016 8:49 am
Subject: [TN] Calling All Metallurgists

All:

Thanks for the auger discussions.

Here's another weird one for all of you hardcore metallurgists.

Client has white gold parts covered with 30 micro inches of gold plating.

White gold is Au-60%, Pt 11%, Cu 14%, Ag 7%, Zn 1.5% and Pd 6.5%.

They would like to remove the flash gold ....ideas?

Thanks


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________
-- 
Bob Wettermann
BEST Inc



-- 
Bob Wettermann
BEST Inc
[log in to unmask]
Cell: 847-767-5745

ATOM RSS1 RSS2