Paul:
What would the preheat be?
Regards,
Ramon
> -----Original Message-----
> From: Stolar, Paul W [SMTP:[log in to unmask]]
> Sent: Thursday, August 28, 2003 9:28 AM
> To: [log in to unmask]
> Subject: Re: [TN] Cracking Ceramic SMT Capacitors
>
> Is your preheat correct. We eliminated our shorting/cracked caps by
> improving our preheat process for Reflow.
>
>
>
> Paul Stolar
>
> Materials Engineer
>
> Houston Technology Center
>
> Baker Atlas
>
> 713-625-5376
>
> 713-625-4949 (fax)
>
> -----Original Message-----
> From: Bob Perkins [mailto:[log in to unmask]]
> Sent: Wednesday, August 27, 2003 6:42 PM
> To: [log in to unmask]
> Subject: [TN] Cracking Ceramic SMT Capacitors
>
>
>
> Cracking Ceramic SMT Capacitors
>
>
>
> " Is anyone else seeing an increase in the number of cracked and shorting
> ceramic chip capacitors? In our experience as a contract manufacturer we
> have, in the past, seen the occasional instance of ceramic capacitors
> cracking and shorting out. The cause of this problem is generally obvious,
> as it is isolated to components situated in areas of the PCB that are
> subject to flexing.
>
>
>
> Recently however we have seen more frequent instances of this problem;
> very often in areas of the board that should not be experiencing any
> appreciable flex. Our process has not changed and neither have our sources
> of these components. Have chip capacitors themselves become more fragile?"
>
>
>
>
> Rod Lafond
>
> Manager, Quality Assurance and Technical Training
>
> APEX-Micro Manufacturing Corporation
>
> [log in to unmask] <mailto:[log in to unmask]>
>
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|