TECHNET Archives

June 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Dudi Banitt <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 25 Jun 1998 08:09:33 +-300
Content-Type:
multipart/mixed
Parts/Attachments:
text/plain (1272 bytes) , application/ms-tnef (2167 bytes)
Dave
You can use the same markers used in AOI for marking the boards, it seems they do the job and are pretty well removable.
David Banitt
----------
From:   Dave Pick -"process engineer"[SMTP:[log in to unmask]]
Sent:   יום חמישי, יוני 25, 1998 03:10
To:     [log in to unmask]
Subject:        [TN] defect marking

I am looking for a temporary way to mark defects on a PCB assembly (other than
the red arrows that everyone uses). The boards will go back through a water
wash, so I was thinking a water soluable, non-conductive ink would be nice. Are
there any recommendations?

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################





ATOM RSS1 RSS2