iNEMI stimulate standard setting, but do not set them... IPC set the
standards... based on my limited understanding (see attached mission
statements for both)...I am not sure both orgnization should have the
consistant view on any particular issues.. specifically, fuzzy issues...
jk (my low cost 1.72 cents)
"The International Electronics Manufacturing Initiative (iNEMI) is an
industry-led consortium whose mission is to assure leadership of the global
electronics manufacturing supply chain. With a membership that includes
approximately 70 electronics manufacturers, suppliers, associations,
government agencies and universities, iNEMI provides an environment in which
partners and competitors alike can collectively anticipate future technology
and business needs and effectively develop collaborative courses of action
to meet those needs.
iNEMI roadmaps the needs of the global electronics industry, identifies
technology and infrastructure gaps and helps eliminate those gaps (both
business and technical) through:
accelerated deployment of new technology
development of industry infrastructure
dissemination of efficient business practices
stimulation of standards
iNEMI also works with government, universities and other funding agencies to
set priorities for future industry needs and R&D initiatives."
=======
Since 1957, IPC-Association Connecting Electronics IndustriesR has been
guiding the electronic interconnection industry through its dramatic
changes. A global trade association dedicated to the competitive excellence
and financial success of its more than 2, 300 member companies, IPC is the
only electronic interconnect organization that brings together all industry
players, including designers, board manufacturers, assembly companies,
suppliers, and original equipment manufacturers.
As a member-driven organization and leading source for industry standards,
training, market research and public policy advocacy, IPC supports programs
to meet the needs of a $40 billion U.S. industry that employs more than
350,000 people. The Association also provides its members with countless
opportunities to network-the ultimate renewable resource and a cornerstone
of IPC membership since day one-through its international tradeshows,
educational programs, technical conferences and online seminars.
====
abcd
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Wayne Thayer
Sent: Tuesday, December 19, 2006 11:55 AM
To: [log in to unmask]
Subject: [TN] Fwd: RE: [TN] iNEMI Hi rel Pb-free finish report
George-
Thanks for considering this issue.
Yes, I did review that UL paper prior to bringing this up on TechNet.
And I apologize for my misleading, non-technical language like
"decriminalize" and "pressure". But I think that, because of the title
of Section VIII of the report, which is about PCBs, that the iNEMI
report considers circuit boards a "component" covered by their
recommendations.
Please allow me to re-state my question in a more presentable form:
The recent iNEMI report contains phrases such as
from page 6, section IIIC: Finishes that Should Generally be Avoided
(in no particular order)
"9. Silver finishes are not prone to whisker growth in most
environments. However, rapid growth of silver dendrites or, in some
cases, silver whiskers may form in the presence of H2S (found in some
cases where the environmental air pollution contains SO2). Additionally,
users sometimes avoid silver finishes due to potential issues with
electromigration and solderability shelf life."
and from section VIII: Printed Circuit Boards:
"Of these surface finishes, immersion tin is susceptible to the
formation of pure tin whiskers and immersion silver is susceptible to
the formation of silver sulfide dendrites."
There are other sections in the paper which also place ImAg in a light
not commensurate with the published data I have reviewed.
Anyway, has anyone seen actual data which supports these statements?
The UL paper you and I both found suggests that ImAg is no more
susceptible to electrochemical migration (I hear you Bev!) than most
other finishes. The subject paper contains language which gives me the
impression some hydrogen sulfide tests were done with ImAg and the
results were of concern, but the only obviously relevant paper in the
reference area was
38 Chudnovsky, Bella, "Degradation of power Contacts in Industrial
Atmosphere: Silver Corrosion and Whiskers". Proceedings of the 48th IEEE
Holm Conference on Electrical Contacts, 2002
which I don't have ready access to, but I suspect it doesn't concern
ImAg.
Wayne
>>> "Wenger, George M." <[log in to unmask]> 12/18/2006 9:05:26
pm >>>
Wayne,
I'll take a stab at answering the two questions you raised and also
correct one of the statements you made.
You indicated incorrectly that you "know that UL recently
"de-criminalized" ImAg, primarily based on IPC pressure." The IPC
didn't pressure UL to "de-criminalize" immersion silver. IPC member
companies who had experience with immersion silver surface finish on
PCBs jointed the IPC 3-11g sub-committee along with UL participation
and
generated data that resulted in UL update the testing requirements
that
were being imposed on silver finishes. IPC and UL are organizations
that make specification changes based on data not pressure.
As for why iNEMI hasn't "de-criminalized" there was no reason for them
to "de-criminalize" immersion silver because they had never
"criminalized" it. If you look at the title of the paper written by
the
iNEMI Tin Whisker User Group it covers "iNEMI Recommendations on
Lead-Free Finishes for Components Used in High-Reliability Products".
This group concentrated on component finishes not board finishes. In
particular, if you look at Table 5 in their report that summarizes the
assessments of the individual members of the iNEMI Users Group
relative
to PCB finishes you will see that there are no tin whisker test
requirements for immersion silver.
As for papers on the electro-migration severity of immersion silver I
would start on the UL PCB site:
http://www.ul.com/pwb/silver.html
and then review the IPC 3-11g committee work.
Regards,
George
George M. Wenger
Andrew Corporation Wireless Network Solutions
Senior Principal FMA / Reliability Engineer
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 [Office] (732) 309-8964 [Cell]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer
Sent: Monday, December 18, 2006 3:48 PM
To: [log in to unmask]
Subject: Re: [TN] iNEMI Hi rel Pb-free finish report
Sorry. Here you go:
http://thor.inemi.org/webdownload/projects/ese/tin_whiskers/Pb-Free_Finishes
_v4.pdf
Wayne
>>> [log in to unmask] 12/18/2006 2:57:21 pm >>>
Is the iNEMI 12/1/06 Pb-Free finish report published some
Wayne,
Is the iNEMI 12/1/06 Pb-Free finish report published somewhere?
Regards,
George
George M. Wenger
Senior Principle FMA / Reliability Engineer
Wireless network Solutions
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908)
546-4531
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer
Sent: Monday, December 18, 2006 2:50 PM
To: [log in to unmask]
Subject: [TN] iNEMI Hi rel Pb-free finish report
In this report (dated 12/1/06) there are several cautions about
Immersion Ag due to electro-migration issues, particularly in
sulfurous
environments.
I know that UL recently "de-criminalized" ImAg, primarily based on IPC
pressure. Why hasn't iNEMI?
Can anybody recommend a paper which explains the severity of this
electro-migration issue with respect to ImAg?
Thanks,
Wayne Thayer
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------
------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------
------------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------
----------------------------------------------------------------------------
--------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
----------------------------------------------------------------------------
--------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|