TECHNET Archives

May 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Andy Magee <[log in to unmask]>
Date:
Mon, 24 May 1999 21:59:25 -0400
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
Parts/Attachments:
text/plain (51 lines)
There have been many helpful comments on this already, so at the risk of
being redundant here are just a couple more:

Probably the most commonly used micro-etch for copper is ammonia /
peroxide which is easy to get, simple to make up (but it must be freshly
made each time) and is fairly harmless to work with.

Metallography on thin copper is a bit of an art. Labs that do it all the
time know the pitfalls, but heed Werner's warning against using just any
lab. The apparent grain structure can be changed significantly by the
act of preparing the sample itself.

While classic copper annealing is done at relatively high temperatures
(600F), it's possible to anneal wrought copper foil at temperatures as
low as 325F in a couple of hours. (The difference being made up by the
residual energy stored in the grains during the rolling process.) This
depression of the annealing time & temperature is typically designed in
by the foil manufacturer to suit the needs of the printed circuit
industry and matches well with common lamination cycles. In most cases
recrystallization only occurs at temperatures above 700F.

Andy Magee
Flex Guru - Consulting
[log in to unmask]
(937) 435-3629

ps. Yes, among other things I have an MS in Metallurgy.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2