TECHNET Archives

March 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Brad L. Matthies" <[log in to unmask]>
Date:
Fri, 31 Mar 2000 16:18:45 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Edward J. Valentine" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Edward J. Valentine" <[log in to unmask]>
Parts/Attachments:
text/plain (64 lines)
BLM -

Although I couldn't find it in the new IPC-SM-782 (Surface Mount Land
Patterns), the old, original version of 782 (March 1987) had the spacing at
0.025" (0.63mm), via pad to smt pad on page 65.  Ed/

Ed Valentine
Electronics Manufacturing Solutions
8612 Mourning Dove Road, Raleigh, NC 27615
Phone: (919) 270-5145, Fax: (919) 847-9971
Email: [log in to unmask]
Website: http://www.ems-consulting.com

----- Original Message -----
From: Brad L. Matthies <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, March 31, 2000 1:27 PM
Subject: [TN] Via Hole Placement.


> TN,
>
> We are experiencing some manufacturing problems (solder bridging) and
> have linked them to via hole placement.  The particular assembly we are
> manufacturing has multiple via holes that are within approximately 15
> Mils of SMT lands.  Does anyone have a resource that spells out safe
> distances of via holes to SMT lands that they can pass along?  We are
> getting ready to approach the design group for this product and are
> looking for a qualified resource of information that we can use as well
> as the design group.
>
> Thanks,
> BLM
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2