TECHNET Archives

May 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"McGlaughlin, Jeffrey A" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, McGlaughlin, Jeffrey A
Date:
Thu, 22 May 2008 14:04:11 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (68 lines)
Kenny -

Wouldn't that be dictated by the calibration of your SG test equipment?
As an amateur vintner my gauge for SG of wine is calibrated for 68
Degrees F. There is an adjustment factor for each degree of variation
above calibration temperature, and a separate factor for each degree
below calibration temp.  Since SG is a relative measure to water a STP
it would make sense (to me at least) to normalize all measurements to
that. 


Jeffrey McGlaughlin, CID 
Engineering Designer 
Battelle 
505 King Avenue 
Columbus Ohio 43201-2693 
(614)424-7582 Phone 
(614)458-7582 Fax 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Thursday, May 22, 2008 1:30 PM
To: [log in to unmask]
Subject: [TN] Specific Gravity for ROSE Tester

Good Day All,

We are having a discussion about the specific gravity of the 75%/25%
solution in our ROSE tester. The question revolves around testing it hot
or
cold.

Our ROSE tester runs at 112 degrees F and would like to know whether we
should test the SG at hot or cold. If so what would we expect for a
reading?

Thanks all,

KennyB

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2