Are you sure it is not a die change that just fails the spec limits of the ICT? What type of test is it failing?
Blair Hogg
>>> [log in to unmask] 07/24/03 01:36PM >>>
Hi all!
We've been building an assembly here for quite a while, and just recently
experienced quite a bit of failures at ICT with one IC. Out of 50 assemblies,
only 3 passed. The failures on the rest of them have been with one IC at the same
location.
I've x-ray'ed the failed parts and don't seen any broken or missing wire
bonds, so I wanted to take a look at the die area to see if I could spot something
obvious.
-Steve Gregory-
**********************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they
are addressed. If you have received this email in error please notify
the system manager.
This footnote also confirms that this email message has been swept
for the presence of computer viruses.
www.hubbell.com - Hubbell Incorporated
**********************************************************************
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------