     Hello,
        What methods are people using to measure line widths after etch on 
     innerlayers. The copper weight can be 0.5 to 1 oz. The trace width can 
     be 2 to 10 mils. The current method is too slow. An operator uses a 
     video inspection system. He manually puts the piece on the table, 
     lines it up and uses knobs to align reticules on a screen with the 
     image. 
        Is anyone using things like electrical tests, controlled impedance, 
     TDR?  What about laser edge detection systems? What kind of automation 
     is available?
     Thanks
     Rich Olsen
------------------------------------------------------------------
     Richard Olsen                Telephone (602)-232-9154
     Continental Circuits Corp.   Main      (602)-268-3461
     3502 East Roeser Road        Fax       (602)-268-0208
     Phoenix Arizona              Pager     (602)-310-6245
     85040-2905                   Internet  [log in to unmask]
     USA                    I make circuit boards,what do you do?
------------------------------------------------------------------
     
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2