Dennis Ward wrote:
>
> Good morning everyone,
>
> Hope everyone had a great New years. Quick
> question. On a 18 X 24 panel what is the maximum
> size of an individual board and still get TWO boards
> per panel? Please no "contact your board vendor"
> replies. I have documentation for four different
> vendors and each has something different. And I
> understand that each will be different. I am curious
> how these vendors stack up with the rest of the
> industry. I've seen sizes from 16.00 X 10.90
> (the smallest) to 16.50 X 11.20 (the largest).
>
> What is realistic? Is the 16.00 X 10.90 too
> conservative and the 16.50 X 11.20 too large??
>
> Thanks for the replies
> Dennis
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
Hi Dennis,
16.5 X 11.2 is possible with no fabrication issues. This is based on
leaving a .75 X .75 boarder of thiefing and a .1 rout separation between
the pieces.
The .75 X .75 is necessary for plating clamping and possible post
etch punch. If these boards were double sided you could actually squeeze
larger pieces on the board.
If the boards were square, ( at least on one edge ) you could gain
another .1 back by scoring instead of routing. Hope this helps!
Regards,
David G. Pacheco
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|