Hi Andre! I would suggest you get a Scanning Electron Microscopy element
scan conducted on the white residue. The white residue you describe could
be tin or lead oxides, lead crystals due to a component plating problem,
calcium crystals due to poor washing, etc. The SEM analysis will help
eliminate the inorganic (e.g. metallic) possibilities leaving the possible
flux related (organic) source causes. Good luck and Happy Holidays.
Dave Hillman
Rockwell Collins
[log in to unmask]
Andre Leclair <[log in to unmask]>@ipc.org> on 12/19/2001 07:57:26 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] white powder on leads
Hi All
Here is another residue issue
We have an assembly which has a white residue remaining after wash.
The board is completely SMT (WS609) using a DI-Wash process, the board is
spotless except for one location. The location is a QFP (from CRONTEL),
the white powder is on the leads of the IC only. There is not a spot on
the PCB.
The Powder dry brushes extremly easily. On a few of the leads ( usually
about half way up the lead, nver near the joint)after brushing there is
evidence of flux residue( yellow sort of like Crystal Flux residue) in
spots.
We have put a few boards through the Omega with readings lower then
2.3microgram/sq.inch.
Could this be something the part manufacture has left/put on the leads? I
have noticed that the plating is thin on the leads (exposed copper on the
faces) the leads also look like sheared stock ( exposed copper on the
sides)
Thanks
Andre
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|