TECHNET Archives

November 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Wed, 31 Oct 2001 22:49:32 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
In-Reply-To:
<013401c1623b$89cfbd10$6401a8c0@kramer>
Content-Type:
text/plain; charset="us-ascii"
From:
Parts/Attachments:
text/plain (40 lines)
Hello,

I would like to ask your input on trouble shooting a wave soldering
process that I've encountered producing blow holes on the PCA. The blow
holes were seen at random locations, mostly on small and light caps. The
boards were manufactured in recent weeks. Some board warppage was
noticed after the wave.

Things I tried:
- Boards from a different manufactured date, no effect
- Turned on turbulence wave. It reduced but didn't completely eliminate
the defect
- used stiffener on board edge to reduce board sagging
- used dummy weights on top of parts seen having defect to minimize
"dancing" during wave

How critical is the component lead-to-hole ratio as far as its impact on
solder joint quality?
Could anyone explain how a blow hole can occur and possible steps taken
to eliminate the defect?

Rgds,
Peter



_________________________________________________________
Do You Yahoo!?
Get your free @yahoo.com address at http://mail.yahoo.com

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2