TECHNET Archives

October 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Marsico, James" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 1 Oct 2003 11:07:23 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (75 lines)
Judy,  One word of caution.  If you ever have to remove the BGA for any
reason, and have to clean up the PWB, chances are that you might damage (or
completely remove) the solder mask on the dog bone pattern.  I would suggest
moving the ground layer to layer 2 and have "pads only" on layer 1.

Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879


        -----Original Message-----
        From:   Kile, Judy K (MED) [SMTP:[log in to unmask]]
        Sent:   Tuesday, September 30, 2003 5:11 PM
        To:     [log in to unmask]
        Subject:        [TN] BGA780 tied directly to gnd plane

        Hello,
        I am looking for potential issues with a proposed design "solution"
on a
        780pin BGA.

        Reason for this approach
        1.) reduce ground bound to this BGA by tying unused pins to gnd
        2.) minimize routing layers

        Proposed solution for the 1mm 780 BGA is to tie the BGA pads
directly to

        a gnd plane (top side assembly & plane) very similar to the dog bone
        pattern.
        The thermal tie will be 1 "spoke" and covered with soldermask.

        There is ~25-30 unused pins that would be tied in this manner.

        ???
        1.) What are the potential assembly issues with solution?
        2.) Are there any reliability issues long term?
        3.) Are there other issues with this design proposal?

        Thanks for your advice,

        Judy Kile
        Global Electrical Technology Center
        Phone: 262-548-2241
        Fax: 414-908-9584

        ---------------------------------------------------
        Technet Mail List provided as a service by IPC using LISTSERV 1.8e
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
        To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
        Search the archives of previous posts at:
http://listserv.ipc.org/archives
        Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
        -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2