FR-4 is a fire retardant woven glass epoxy substrate. Getek, a trade name,
is a similar product using PPO epoxy in place standard epoxy resin.
Polyimide is a replacement resin for the epoxy still using woven glass.
Teflon is a trade name for PTFE plastic it is used with a number of fillers
to create a substrate. Rodgers is a manufacturer who produces all or most of
the above plus a line of thermo set plastic laminates used for pcb
manufacture. For more specific answers on the properties of these materials
see IPC-4101.
Jeffrey A. McGlaughlin, C.I.D.
Sr. PCB Designer
Battelle Memorial Institute
Columbus Ohio
[log in to unmask]
-----Original Message-----
From: KUMAR [mailto:[log in to unmask]]
Sent: Monday, February 19, 2001 12:11 PM
To: [log in to unmask]
Subject: [TN] materials
hello,
whats the difference between the materials fr4, gtec, rogers,
polymide & teflon ?
thanx
kumar
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|