Royce, Here are a few suggestions...
Tombstoning Mitigation Techniques:
. Use a larger width and area of metallization under the chip
component
. Use adequate spacing between the two pads of the chips
. Use a proper extension of the solder pad beyond the chip ends.
Circular pads appear to be more promising than rectangular or square pads
. Reduce the width of the solder pads
. Minimize the uneven distribution of thermal mass, including the
connection of pads with heat sinks
. Minimize the shadow effect through adequate design of PCB and
selection of reflow methods
. Use organic solderability preservatives or nickel/gold coating or Sn
coating instead of Sn/Pb coating on copper pads
. Reduce the contamination or oxidation level of the component
termination metallization or PCB pad metallization
. Use a thinner paste print thickness
. Improve component placement accuracy
. Use a milder heating rate at reflow
. Avoid using vapor phase reflow method
. Pre-dry the paste before reflow or use a profile with a long soaking
zone to reduce the Outgassing rate of the fluxes
. Use solder paste with retarded melting temperature or with a wide
pasty range (Indalloy #100: Anti-Tombstoning Alloy offered by Indium
Corporation)
. Use a profile with a very slow ramp rate across the melting
temperature of the solder
Christopher J. Nash
Indium Corporation of America
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Royce Taylor
Sent: Monday, January 15, 2007 2:04 PM
To: [log in to unmask]
Subject: [TN] tombstoning of 0508 ceramic capacitors
I have a question for the "Adhesive Dispense" OR the "0508 chip" experts
out in Technet land.
We at times struggle with 0508 capacitors tombstoning (yes, 0508 not
0805). We do run Nitrogen and turning it off helps at times but there are
many times we need to run nitrogen for other reasons. Most times we try to
dispense a dot of adhesive (Loctite 3609) but we are having occasional
issues with the adhesive getting into the solderpaste, the gap between the
pads measures ONLY 0.020" so it is difficult to prevent this from
happening. Does anyone out there run into the same issues?? Any
thoughts?? We run a Camalot Gemini and a Fuji GL dispenser and use a 25 GA
needle. Also we use Indium SMQ92J No Clean solderpaste so I don't know if
this paste is contributing to the tombstoning.
A re-layout of the boards is not an option. We have tried both a "straight
ramp" and a "ramp-soak-ramp" profile with little or no difference.
Thanks for your thoughts and advice
Royce
*************************************************
Royce Taylor
Raytheon
350 Lowell St.
Andover, MA 01810
(978) 470-7431
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|