TECHNET Archives

May 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 5 May 2004 10:46:56 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Steve Gregory <[log in to unmask]>
Parts/Attachments:
text/plain (30 lines)
Hi Charles!

Finally got your pictures up. Go to: http://www.stevezeva.homestead.com and
look at "Green Residue 1 and 2". Looking at the pictures, it sure looks like
something is reacting with the copper. Maybe some flux got accidently splashed
or spilled on the board after it was cleaned. How many assemblies exhibit this
problem?

-Steve Gregory-


> When we do the hand solder it takes about 1.5 hr. so we clean with IPA then
> wash with water. The flux core is alcohol based and cleans fairly well with
> IPA but we do hand clean after with saponifier and water. I did a little
> experiment with new copper. It looks like it might be the WS flux, but the
> parts that have the green are not hand soldered and the parts that are hand
> soldered do not have it.
>


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2