Ken Patel <[log in to unmask]>
Date:
Tue, 25 Jan 2005 14:17:01 -0800
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>, David Tremmel <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ken Patel <[log in to unmask]>
Parts/Attachments:
text/plain (101 lines)
All,
As we don't have compressed air in the building, I have been asked to find
out - Is there any vacuum sealer that does not need compressed air?

Re,
Ken Patel

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Tremmel
Sent: Friday, January 21, 2005 1:20 PM
To: [log in to unmask]
Subject: Re: [TN] Vacuum Sealer

James,

Can you send me the Model Number?

Thank you,

David

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Cagle, James
Sent: Friday, January 21, 2005 3:17 PM
To: [log in to unmask]
Subject: Re: [TN] Vacuum Sealer

We have a bench-top by AmeriVac that works well and fairly cheap. We just
use shop air.
James Cagle
Tycoelectronics


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ken Patel
Sent: Friday, January 21, 2005 12:36 PM
To: [log in to unmask]
Subject: [TN] Vacuum Sealer


Any suggestion on vacuum machine for resealing of ESD component bags?



Re,

Ken Patel


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2