Gregg,
As a general rule...NO, you do not have to worry about gold
embrittlement when using gold plated boards.
99.9999% of gold boards are ENIG which has negligible amounts of gold.
As others have already mentioned, electroplated gold is a different
story and one does need to be careful. However, electroplating does not
happen by accident. You have to go to the extra trouble and
specifically design for and request the thicker gold. Then the board
shop will likely try to talk you out of it unless you insist.
-Ryan Grant
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gregg A. Owens
Sent: Wednesday, December 01, 2004 12:23 AM
To: [log in to unmask]
Subject: [TN] Gold Plated Board
Dear TechNetters,
One of my students has a good question, I can't answer. J-STD-001
requires gold removal of various gold plated components/terminals. What
if you are using a gold plated board plating. Is there generally any
problems with gold embrittlement with this type of board plating with
non-gold plated leads for through-hole or SMT components?
Your thoughts would be most appreciated.
Gregg A. Owens
Manufacturing Technology Training Center, Inc.
Mira Loma, CA 91752 USA
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|