TECHNET Archives

January 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Sat, 27 Jan 2007 14:10:54 EST
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="UTF-8"
From:
Werner Engelmaier <[log in to unmask]>
Parts/Attachments:
text/plain (39 lines)
Hi Andrew,
That FAB note has a number of shortcomings.
"Construction to be SMOBD, using liquid photoimageable (LPI) solder mask
material, type XXXX. Apply to both external layers in accordance with IPC,
(Type B, Class 2). Use appropriate solder mask artworks for each side of
board."
I would thing SMOBD should be SMOBC.
I have never heard of a solder mask material Type "anything;" why put 
anything like this "down" if it does not have an accepted technical meaning?
"...in accordance with IPC" is meaningless without giving an IPC document 
number—IPC-D-325 is a 'documentation' document; for specification purposes you 
should be using IPC-SM-840.
(Type B, Class 2) also do not correspond to any accepted way of specifying 
solder mask.

I would recommend a FAB Note like this: 
"SOLDER MASK OVER BARE COPPER ACCORDING TO IPC-SM-840, CLASS H, TYPE LIQUID 
PHOTO IMAGEABLE (LPI), 0.0015 MAX THICKNESS, COLOR: GREEN, BOTH SIDES OF THE 
BOARD.   ALL FIDUCIALS, LANDS AND HOLES, EXCEPT VIAS, SHALL BE FREE OF SOLDER 
MASK MATERIAL."

If you are in the process of wring a specification document for your PCBs, my 
White Paper in the subject may be helpful—I am sending the details in a 
separate e-mail.



Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2